Not rated yet

This collection explores all aspects of metallurgical processing, materials behavior, and microstructural performance for the distinct class of 718-type superalloys and derivatives.

Media Books     Hardcover Book   (Book with hard spine and cover)
Released September 4, 2026
ISBN13 9783032351753
Publishers Springer Nature Switzerland AG
Pages 764
Dimensions 150 × 220 × 20 mm   ·   1.26 kg
Editor Andersson, Joel
Editor Bi, Zhongnan
Editor Dempster, Ian
Editor Detrois, Martin
Editor Fahrmann, Michael
Editor Kirka, Michael
Editor Klemm-Toole, Jonah
Editor Ott, Eric A.
Editor Sudbrack, Chantal
Editor Wessman, Andrew

More from the same publisher